Electrocorindón normal 14A
Grano: F012 F014 F016 F020 F022 F024 F030 F036 F040 F046 F054 F060 F070 F080 F090 F100 F120 F150 F180 F220
Composición química %
Al2O3 _ _ _ | ≥95,0% |
Fe2O3 _ _ _ | ≤0,30% |
SiO2 _ | ≤1,00% |
TiO2 _ | 1,7-3,4% |
Alto | ≤0,42% |
Propiedades físicas: electrocorindón normal 14A
Gravedad específica | Gravedad específica |
Dureza de Mohs | 9.0 |
Densidad a Granel | 1,53-1,99 g/cm3 |
Punto de fusion | 2250℃ |
Obstinación | 1900℃ |
PSD (distribución del tamaño de partículas) del electrocorindón normal 14A
F012 | +2800um | 0 | +2000um | ≤20% | +1700um | ≥45% | +1700+1400um | ≥70% | -1180um | ≤3% |
F014 | +2360um | 0 | +1700um | ≤20% | +1400um | ≥45% | +1400+1180um | ≥70% | -1000um | ≤3% |
F016 | +2000um | 0 | +1400um | ≤20% | +1180um | ≥45% | +1180+1000um | ≥70% | -850um | ≤3% |
F020 | +1700um | 0 | +1180um | ≤20% | +1000um | ≥45% | +1000+850um | ≥70% | -710um | ≤3% |
F022 | +1400um | 0 | +1000um | ≤20% | +850um | ≥45% | +850+710um | ≥70% | -600um | ≤3% |
F024 | +1180um | 0 | +850um | ≤25% | +710um | ≥45% | +710+600um | ≥65% | -500um | ≤3% |
F030 | +1000um | 0 | +710um | ≤25% | +600um | ≥45% | +600+500um | ≥65% | -425um | ≤3% |
F036 | +850um | 0 | +600um | ≤25% | +500um | ≥45% | +500+425um | ≥65% | -355um | ≤3% |
F046 | +600um | 0 | +425um | ≤30% | +355um | ≥40% | 355+300um | ≥65% | -250um | ≤3% |
F054 | +500um | 0 | +355um | ≤30% | +300um | ≥40% | +300+250um | ≥65% | -212um | ≤3% |
F060 | +425um | 0 | +300um | ≤30% | +250um | ≥40% | 250+212um | ≥65% | -180um | ≤3% |
F070 | +355um | 0 | +250um | ≤25% | +212um | ≥40% | +212+180um | ≥65% | -150um | ≤3% |
F080 | +300um | 0 | +212um | ≤25% | +180um | ≥40% | +180+150um | ≥65% | -125um | ≤3% |
F090 | +250um | 0 | +180um | ≤20% | +150um | ≥40% | +150+125um | ≥65% | -106um | ≤3% |
F100 | +212um | 0 | +150um | ≤20% | +125um | ≥40% | +125+106um | ≥65% | -75um | ≤3% |
F120 | +180um | 0 | +125um | ≤20% | ≥40% | ≥40% | +106+90um | ≥65% | -63um | ≤3% |
F150 | +150um | 0 | +106um | ≤15% | +75um | ≥40% | +75+63um | ≥65% | -45um | ≤3% |
F180 | +125um | 0 | +90um | ≤15% | +75um | * | +75+63um | ≥40% | -53um | * |
F220 | +106um | 0 | +75um | ≤15% | +63um | * | +63+53um | ≥40% | -45um | * |
Principales aplicaciones del electrocorindón normal 14A
-Abrasivos aglomerados y abrasivos recubiertos.
-Medios de chorro húmedo y seco, esmerilado y pulido, etc.
-Voladura de placa PCB (PCBA, FPC, LED)
-Cera para pulir, piedras de amolar, almohadillas para pulir, etc.
-eliminación de incrustaciones, óxido y revestimientos viejos.
-formas de cerámica
-Muelas abrasivas, muelas de copa, etc.
-forros de freno y fricción
…
Embalaje
BOLSAS PVC 25KGS | BOLSA GRANDE DE 1MT | BOLSAS DE PVC DE 25 KG + BOLSA GRANDE DE 1 MT | BOLSAS PVC 25KGS+PALLET |
Pureza de otros grados Electrocorindón Normal 14A
Calificación | Al2O3% |
B | 85-92% |
C | 70-80% |
D | 60-70% |
Y | 50-60% |